Utilization of Microalloying with Rare Earth Elements and Hot Extrusion for Remarkable Grain Refinement and Enhancement of Mechanical Properties of as-Cast Magnesium Alloy
الموضوعات :Hooman Abedi 1 , Massoud Emamy 2 , Hamed Mirzadeh 3 , Jafar Rassizadehghani 4 , M. Ra'ayatpour 5
1 - School of Metallurgy and Materials Engineering, College of Engineering, University of Tehran, P.O. Box 11155-4563, Tehran, Iran
2 - School of Metallurgy and Materials Engineering, College of Engineering, University of Tehran, P.O. Box 11155-4563, Tehran, Iran
3 - School of Metallurgy and Materials Engineering, College of Engineering, University of Tehran, P.O. Box 11155-4563, Tehran, Iran
4 - School of Metallurgy and Materials Engineering, College of Engineering, University of Tehran, P.O. Box 11155-4563, Tehran, Iran
5 - School of Metallurgy and Materials Engineering, College of Engineering, University of Tehran, P.O. Box 11155-4563, Tehran, Iran
الکلمات المفتاحية: Mechanical Properties, Recrystallization, Mg alloys, Ultrafine grained microstructure,
ملخص المقالة :
The effects of micro-addition by rare earth (RE) elements (via cerium-based mischmetal) and hot deformation (via extrusion process) on the microstructure and mechanical properties of Mg-0.5Zn-0.5Zr alloy were studied. Optical microscopy, scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), and tensile testing were used for characterization of alloys in the as-cast and wrought conditions. It was found that the addition of 0.5 wt% RE combined with the hot extrusion process could remarkably refine the grain size from 1320 µm for the as-cast Mg-0.5Zn-0.5Zr alloy to the recrystallized grain size of 1.3 µm for the extruded Mg-0.5Zn-0.5Zr-0.5RE alloy. Compared to the as-cast counterparts, the ultimate tensile strength (UTS) and total elongation to failure were significantly enhanced by the extrusion process. Quantitatively, the UTS of ~ 300 MPa with the total elongation of ~ 18% was obtained for the extruded Mg-0.5Zn-0.5Zr-0.5RE alloy, which reveals the favorable effects of the ultra grain refinement on the enhancement of the mechanical properties of magnesium alloys.
[1] Ö. Ayer, Effect of die parameters on the grain size, mechanical properties and fracture mechanism of extruded AZ31 magnesium alloys, Materials Science and Engineering A 793 (2020) 139887.
[2] S. Lv, F. Meng, X. Lu, Q. Yang, X. Qiu, Q. Duan, J. Meng, Influence of Nd addition on microstructures and mechanical properties of a hot-extruded Mg− 6.0 Zn− 0.5 Zr (wt.%) alloy, Journal of Alloys and Compounds 806 (2019) 1166-1179.
[3] M.M. Hoseini-Athar, R. Mahmudi, R.P. Babu, P. Hedström, Effect of Zn content on the microstructural stability and grain growth kinetics of fine-grained extruded Mg–Gd–Zn alloys, Journal of Alloys and Compounds 831 (2020) 154766.
[4] I. Dinaharan, S. Zhang, G. Chen, Q. Shi, Development of titanium particulate reinforced AZ31 magnesium matrix composites via friction stir processing, Journal of Alloys and Compounds 820 (2020) 153071.
[5] J. Deng, Y.C. Lin, S.S. Li, J. Chen, Y. Ding, Hot tensile deformation and fracture behaviors of AZ31 magnesium alloy, Materials and Design 49 (2013) 209-219.
[6] M.A. Easton, M. Qian, A. Prasad, D.H. StJohn, Recent advances in grain refinement of light metals and alloys, Current Opinion in Solid State and Materials Science 20 (2016) 13-24.
[7] A.H. Blake, C.H. Cáceres, Solid-solution hardening and softening in Mg–Zn alloys, Materials Science and Engineering A 483 (2008) 161-163.
[8] F. Sayari, R. Mahmudi, R. Roumina, Inducing superplasticity in extruded pure Mg by Zr addition, Materials Science and Engineering A 769 (2020) 138502.
[9] A. Hadadzadeh, M.A. Wells, Analysis of the hot deformation of ZK60 magnesium alloy, Journal of Magnesium and Alloys 5 (2017) 369-387.
[10] K Guan, F Meng, P Qin, Q Yang, D Zhang, B Li, W. Sun, S. Lv, Y. Huang, N. Hort, J. Meng, Effects of samarium content on microstructure and mechanical properties of Mg–0.5Zn–0.5Zr alloy, Journal of Materials Science and Technology 35 (2019) 1368-1377.
[11] M. Yuan, Z. Zheng, Effects of Zn on the microstructures and mechanical properties of Mg–3Sm–0.5 Gd–xZn–0.5 Zr (x= 0, 0.3 and 0.6) alloy, Journal of Alloys and Compounds 590 (2014) 355-361.
[12] S. Wang, W. Zhang, H. Wang, J. Yang, W. Chen, G. Cui, G. Wang, Microstructures evolution, texture characteristics and mechanical properties of Mg-2.5 Nd-0.5 Zn-0.5 Zr alloy during the high strain rate hot-rolling, Materials Science and Engineering A (2020) 140488.
[13] M. Zhang, J. Zhao, M. Chen, Comparative study of the effects of CaO and Ce-La misch metal on the microstructure and properties of AZ91 alloy, Journal of Materials Research and Technology 9 (2020) 5194-5203.
[14] M. Golrang, M. Mobasheri, H. Mirzadeh, M. Emamy, Effect of Zn addition on the microstructure and mechanical properties of Mg-0.5Ca-0.5RE magnesium alloy, Journal of Alloys and Compounds 815 (2020) 152380.
[15] Stanford, Nicole, et al. "Effect of microalloying with rare-earth elements on the texture of extruded magnesium-based alloys." Scripta Materialia 59.7 (2008): 772-775.
[16] Huang, Yuanding, et al. "Role of multi-microalloying by rare earth elements in ductilization of magnesium alloys." Journal of magnesium and alloys 2.1 (2014): 1-7.
[17] Fang, Xiaogang, et al. "Effects of Ce/La misch metal content on microstructure evolution and mechanical properties of Mg-Zn-Y alloy." Materials Science and Engineering: A 699 (2017): 1-9.
[18] P. Cao, M. Qian, D.H. StJohn, Native grain refinement of magnesium alloys." Scripta Materialia 53 (2005) 841-844.
[19] S.M. Fatemi-Varzaneh, A. Zarei-Hanzaki, H. Beladi, Dynamic recrystallization in AZ31 magnesium alloy, Materials Science and Engineering: A 456 (2007) 52-57.
[20] S. You, Y. Huang, K.U. Kainer, N. Hort, Recent research and developments on wrought magnesium alloys, Journal of Magnesium and Alloys 5 (2017) 239-253.
[21] Z. Zeng, N. Stanford, C.H.J. Davies, J.F. Nie, Ni. Birbilis, Magnesium extrusion alloys: a review of developments and prospects, International Materials Reviews 64 (2019) 27-62.
[22] T. Al-Samman, G. Gottstein, Dynamic recrystallization during high temperature deformation of magnesium, Materials Science and Engineering A 490 (2008) 411-420.
[23] G. Dieter, Mechanical Metallurgy, 3rd ed., McGraw-Hill, NewYork, 1986.
[24] H. Mirzadeh, High strain rate superplasticity via friction stir processing (FSP): A review, Materials Science and Engineering A 819 (2021) 141499.
[25] B.P. Zhang, L. Geng, L.J. Huang, X.X. Zhang, C.C. Dong, Enhanced mechanical properties in fine-grained Mg–1.0 Zn–0.5 Ca alloys prepared by extrusion at different temperatures, Scripta Materialia 63 (2010) 1024-1027.
[26] B. Pourbahari, H. Mirzadeh, M. Emamy, R. Roumina, Enhanced Ductility of a Fine‐Grained Mg–Gd–Al–Zn Magnesium Alloy by Hot Extrusion, Advanced Engineering Materials 20 (2018) 1701171.