Punch plastic deformation pipe cladding (PPDPC) as a novel tube cladding method
Subject Areas : ChemistryM.R. Baghaei 1 , Ghader Faraji 2
1 - University of Tehran
2 - Department of Mechanical Engineering, College of Engineering, University of Tehran, Tehran, Iran
Keywords:
Abstract :
[1] F. Liu, J. Zheng, P. Xu, M. Xu, and G. Zhu, “Forming mechanism of double-layered tubes by internal hydraulic expansion”, Int. J. Press. Vessel. Pip., vol. 81, no. 7, 2004, pp. 625–633.
[2] N. R. Chitkara and A. Aleem, “Extrusion of axi-symmetric bi-metallic tubes: Some experiments using hollow billets and the application of a generalised slab method of analysis”, Int. J. Mech. Sci., vol. 43, no. 12, 2001, pp. 2857–2882.
[3] J. S. Lee, H. T. Son, I. H. Oh, C. S. Kang, C. H. Yun, S. C. Lim, and H. C. Kwon, “Fabrication and characterization of Ti-Cu clad materials by indirect extrusion”, J. Mater. Process. Technol., vol. 187–188, 2007, pp. 653–656.
[4] Z. Chen, K. Ikeda, T. Murakami, T. Takeda, and J. X. Xie, “Fabrication of composite pipes by multi-billet extrusion technique”, J. Mater. Process. Technol., vol. 137, 2003, pp. 10–16.
[5] X. Sun, J. Tao, And X. Guo, “Bonding properties of interface in Fe/Al clad tube prepared by explosive welding”, Trans. Nonferrous Met. Soc. China, vol. 21, 2011, pp. 2175–2180.
[6] N. Kahraman, B. Gülenç, and F. Findik, “Joining of titanium/stainless steel by explosive welding and effect on interface”, J. Mater. Process. Technol., vol. 169, 2005, pp. 127–133.
[7] K. Bhanumurthy, “Development of tubular transition joints of aluminium/stainless steel by deformation diffusion bonding“, Mater. Sci. Technol., Vol. 22, 2006, pp. 321-330.
[8] Bhanumurthy K, Fotedar R K, Joyson D, Kale G B, Pappachan A L, Grover A K, Krishnan J. “Development of tubular transition joints of aluminium/stainless steel by deformation diffusion bonding“, Mater. Sci. Technol., Vol. 22, 2006, pp. 321-330.
[9] D. L. Sponseller, G. a. Timmons, and W. T. Bakker, “Development of Clad Boiler Tubes Extruded from Bimetallic Centrifugal Castings”, J. Mater. Eng. Perform., vol. 7, 1998, pp. 227–238.
[10] S.-H. Kim, H.-W. Kim, K. Euh, J.-H. Kang, and J.-H. Cho, “Effect of wire brushing on warm roll bonding of 6XXX/5XXX/6XXX aluminum alloy clad sheets” , Mater. Des., vol. 35, 2012, pp. 290–295.
[11] X. Li, G. Zu, Q. Deng, An Investigation of Deformation Behavior of Bimetal Clad Sheets by Asymmetrical Rolling at Room Temperature, Light Metals, 1rd ed., John Wiley & Sons, Inc., 2011, pp. 611.
[12] V. Ocelík and J. T. M. De Hosson, Advances in Laser Materials Processing. 1rd ed., Elsevier, 2010, pp. 157.
[13] X. Wang, P. Li, and R. Wang, “Study on hydro-forming technology of manufacturing bimetallic CRA-lined pipe”, Int. J. Mach. Tools Manuf., vol. 45, 2005, pp. 373–378.
[14] M.A. Spence, C.V. Roscoe, “Bi-metal CRA-lined pipe employed for North Sea field development", Oil Gas J., vol. 97, 1999, pp. 80–88.
[15] Z. L. Zhan, Y. D. He, D. Wang, and W. Gao, “Cladding inner surface of steel tubes with Al foils by ball attrition and heat treatment”, Surf. Coat. Technol., vol. 201, 2006, pp. 2684–2689.
[16] R. Lapovok, H. P. Ng, D. Tomus, and Y. Estrin, “Bimetallic copper-aluminium tube by severe plastic deformation", Scr. Mater., vol. 66, 2012, pp. 1081–1084.
[17] M. S. Mohebbi and A. Akbarzadeh, “A novel spin-bonding process for manufacturing multilayered clad tubes”, J. Mater. Process. Technol., vol. 210, 2010, pp. 510–517.
[18] M. M. Samandari, K. Abrinia, and A. Akbarzadeh, “Production of Bilayer Al / St Tubes by Cold Spin Bonding and Investigation”, vol. 14, 2015, pp. 111–118.
[19] T. Yoshida, S. Matsuda, and S. Matsui, “The development of corrosionresistant Tubing.” Offshore Technol., vol. 2, 1981, pp. 365–378,.
[20] W.C. Chen, C.W. Petersen, “Corrosion performance of welded CRAlined pipes for flowlines", SPE Prod. Eng., vol. 7, 1992, pp. 375–378.
[21] D. K. Russell and S. M. Wilhelm, “Analysis of bimetallic pipe for sour Service.” SPE Prod. Eng., vol. 7, 1991, pp. 291–296.
[22] Internal tube cladding using plastic deformation, Patent no 84006, in persian.
[23] G. Faraji, H.S. Kim, M. M. Mashhadi, “Microstructure inhomogeneity in ultra-fine grained bulk AZ91 produced by accumulative back extrusion (ABE),” Mater. Sci. Eng. A, vol. 528, 2011, pp. 4312–4317.
[24] G. Faraji, P. Yavari, S. Aghdamifar, M.M. Mashhadi, "Mechanical and microstructural properties of ultra-fine grained AZ91 magnesium alloy tubes processed via multi pass tubular channel angular pressing (TCAP)", J. Mater. Sci. & Technol., vol. 30, no. 2, 2014, pp. 134–138.
[25] G. Faraji, M.M. Mashhadi, A.R. Bushroa, A. Babaei, "TEM analysis and determination of dislocation densities in nanostructured copper tube produced via parallel tubular channel angular pressing process", Mater. Sci. Eng. A, vol. 563, 2013, pp. 193–198.